筛选条件 共查询到29条结果
排序方式
Durability of Concrete Incorporating Rice Husk Ashe

期刊: MATERIALS PERFORMANCE, 2019; 58 (3)

Modified rice husk ash (RHA) concrete was prepared by adding different RHA dosages at different ternperatures into cementitious composites. The durabi......

JIF:0.15

Corrosion of 3Cr Steel in Supercritical CO2 Systems

期刊: MATERIALS PERFORMANCE, 2019; 58 (4)

The corrosion behavior of 3Cr steel in static and dynamic water-saturated supercritical carbon dioxide (CO2) systems during carbon capture and storage......

JIF:0.15

Nickel-Rich Coating for Saline-Alkali Soil Grounding

期刊: MATERIALS PERFORMANCE, 2019; 58 (4)

To improve the corrosion resistance of the grounding grids in saline-alkali soil, the authors fabricated a conductive and anticorrosive coating. After......

JIF:0.15

Aluminum Corrosion Influenced by Temperature in Deionized Water

期刊: MATERIALS PERFORMANCE, 2019; 58 (5)

Temperature influence on aluminum corrosion in deionized water was studied using the gravimetric method, optical microscope, and x-ray diffraction. Ac......

JIF:0.15

Failure Due to Cl-SCC of Austenitic Stainless Steels

期刊: MATERIALS PERFORMANCE, 2019; 58 (6)

Corrosion is a foremost problem in many industries. In the petrochemical industry it impacts the equipment and assets of refineries and other faciliti......

JIF:0.15

SCC Inhibition of Super 13Cr in CO2-Saturated CaCl2

期刊: MATERIALS PERFORMANCE, 2019; 58 (8)

The inhibition effect of quinoline quaternary ammonium salt (QQAS) and potassium iodide (KI) on stress corrosion cracking (SCC) of super 13Cr stainles......

JIF:0.15

Salt Spray Corrosion Performances of Amorphous Al-Ti-Ni Coatings

期刊: MATERIALS PERFORMANCE, 2019; 58 (8)

Arc-sprayed amorphous Al-Ti-Ni coatings on S355 structural steel were processed using a laser remelting. The effects of power on the salt spray corros......

JIF:0.15

Corrosion Issues of Carbon Capture, Utilization, and Storage

期刊: MATERIALS PERFORMANCE, 2018; 57 (11)

Carbon capture, utilization, and storage (CCUS) can not only reduce carbon dioxide (CO2) emissions by permanent geological storage but can also enhanc......

JIF:0.15

Formation of Corrosion-Resistant MAO-Treated Aluminum Alloy

期刊: MATERIALS PERFORMANCE, 2018; 57 (2)

Micro-arc oxidation (MAO) coatings were formed on an aluminum alloy in a silicate-based electrolyte with and without the addition of aluminum oxide (A......

JIF:0.15

Durability of Concrete Modified with Superabsorbent Polymers

期刊: MATERIALS PERFORMANCE, 2018; 57 (3)

Ordinary concrete was modified with additions of superabsorbent polymers (SAPs). Research was conducted to assess the weight loss ratio from cyclic fr......

JIF:0.15

Effects of Silane Additives on Corrosion Resistance and Durability of Mortar

期刊: MATERIALS PERFORMANCE, 2018; 57 (3)

Silane coupling agent additives were used in mortar in varying proportions, and the effect of the coupling agent content on the mortar's corrosion cra......

JIF:0.15

FAILURE ANALYSIS: Corrosion of a Reflux Condenser

期刊: MATERIALS PERFORMANCE, 2018; 57 (4)

A reflux condenser used for fluorination production failed after four months of service. Three UNS S30403 stainless steel condenser tubes in this refl......

JIF:0.15

Silane-Zirconium Pretreatment for Mild Steel

期刊: MATERIALS PERFORMANCE, 2018; 57 (4)

An environmentally friendly pretreatment for mild steel, based on silane and zirconium, was developed with the aim of replacing conventional chromatin......

JIF:0.15

Stress Corrosion Cracking Behaviors of Weathering Steel Welded Joints

期刊: MATERIALS PERFORMANCE, 2018; 57 (12)

The changes of stress corrosion cracking (SCC) behaviors in simulated industrial atmospheric environments between weathering steel, 09CuPCrNi, and its......

JIF:0.15

Electrochemical Corrosion Behavior of AA7003

期刊: MATERIALS PERFORMANCE, 2018; 57 (12)

The electrochemical corrosion behavior of 7003 aluminum alloy (AA7003) under peak aging (PA), double peak aging (DPA), and regression re-aging (RRA) i......

JIF:0.15

共29条页码: 1/2页15条/页